Your customer is specifying CEM3 to save $$$ on base material. I will
suggest offering a standard FR4 if CEM3 is not readily available to you
in Taiwan - FR4 exceeds all performance requirements of CEM and can be
used in its place if economics agree. Isola Laminates makes a CM310
material compliant to what your customer needs and I believe is
fabricated in Asia, which maybe available to you:
http://www.isola-usa.com/products/productsbyindustry.shtml
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302-1890
Tel. 802.257.4571.21 Fax. 802.257.0011
[log in to unmask]
http://www.vtcircuits.com
-----Original Message-----
From: Larry Russell [mailto:[log in to unmask]]
Sent: Thursday, September 30, 2004 4:55 AM
To: [log in to unmask]
Subject: [TN] CEM 3 Specs
Technet Sages,
We are moving into mass production shortly on a special order for us,
which has not been around here for ages. The customer wants CEM 3
material, and QA wants to to find out more on the testing
requirements,etc. The IPC literature we have on hand for rigid and flex
does not have much, so where should we be looking?
Appreciatively
Larry Russell
http://www.chantworld.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|