TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Date:
Thu, 16 Sep 2004 12:40:52 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Reeves, Tim R." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Reeves, Tim R." <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
He's saying the board, operating, will be at 75ºC (45ºC env + 30ºC rise from
Joule heating), but the conclusion is still that FR-4, even difunctional,
will be OK at that temperature.

Tim Reeves
Lamination Engineer
Tyco Electronics | Printed Circuit Group | Dallas Division
1270 Monmouth Cutoff Road, Dallas, OR 97338
503.623.1000 Ext.1120


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jeffrey Bush
Sent: Wednesday, September 15, 2004 4:37 AM
Subject: Re: worry about the PCB reliability issue with high
temperature?


30 C is within most FR4 operating temperature of 130 C - a 45 C FR4 is
odd, possible only tested at that range.  Check with your laminate
supplier for operating temperature parameters.  Some difunctional
materials are still at a 40 C OT, with most multifunctional laminates
rated to 130 C. 



Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: minjun 29672 [mailto:[log in to unmask]] 
Sent: Wednesday, September 15, 2004 1:44 AM
To: [log in to unmask]
Subject: [TN] worry about the PCB reliability issue with high
temperature?


hello, Technetters,
Our a product's environmental temperature is 45c, while our power
board's T-rise is about 30c, do you think our PCB (FR4) has reliability
issue with high temp for long term? Any response and suggestion will be
welcome.

Thanks in advance!

Min jun

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2