While I don't disagree with your choice to leave the vias open on one side
or the other, it is a little misleading and shouldn't be used as a general
rule. There are many things to consider, before you can safely implement
that design strategy. Some of them are as follows:
* you have complete knowledge and control of your processes and materials
* You have a very benign end-use environment
* your product is obsolete before it fails
* free replacement is more cost effective than design change
* you make Christmas toys and they only have to work once on Christmas
morning( just make
sure you pick them up before watering the tree and don't put the batteries
in till just
before opening them)
If on the other hand you are making Hi-rel or Aerospace product that you
have to rework and maintain and may not always be in control of your own
destiny, there are only two ways to go. Permanently tent( SMOBC) the vias on
both sides or completely plug and cap( or plate over )to protect the
integrity of the via and provide the long term reliability that is required.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Charles Caswell
Sent: Wednesday, September 15, 2004 7:59 AM
To: [log in to unmask]
Subject: Re: [TN] Question about via masking on BGA pattern...
I can agree to this. I suggested covering both sides just because most of
our
customers question uncovered via's. Not sure why, especially those with
specific notes on drawing to leave via's unplugged and not masked.
-----Original Message-----
From: Jeffrey Bush [mailto:[log in to unmask]]
Sent: Wednesday, September 15, 2004 7:56 AM
To: [log in to unmask]
Subject: Re: [TN] Question about via masking on BGA pattern...
I would recommmend the opposite of this - plug from the BGA side and
leave the bottom open for testing.
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302-1890
Tel. 802.257.4571.21 Fax. 802.257.0011
[log in to unmask]
http://www.vtcircuits.com
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, September 15, 2004 8:44 AM
To: [log in to unmask]
Subject: [TN] Question about via masking on BGA pattern...
Mornin' All!
I have a question about solder masking via's in a BGA pattern, and want
to see if I'm thinking correctly about this.
I think it's a bad idea to leave the via's free from solder mask on the
topside of the board beneath the BGA, and tent the bottomside via's. To
me, you're just asking for trouble down the road because you'll trap
flux residue and all kinds of stuff in the via's that won't be able to
be cleaned out well. This is a 676 ball 1.0mm pitch BGA pattern. Am I
wrong about this?
Thanks!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|