Wei,
I wouldn't worry about the Au not going completely into solution with the
hand soldering of the 0402 caps...
You will probably have more reliability issues with the thermal damage to
the caps, than the Sn-Au and Sn-Ni interfaces...
Paul
Paul Edwards
Process Engineering
[log in to unmask]
Tel: 408-433-4700
FAX: 408-433-9988
Surface Art Engineering
81Bonaventura Dr.
San Jose, CA 95134
DUNS: 944740570
CAGE/NCAGE: 1XZ48
-----Original Message-----
From: Wei-Shun Wang [mailto:[log in to unmask]]
Sent: Monday, September 13, 2004 3:38 PM
To: [log in to unmask]
Subject: [TN] Soldering to hard gold
Hi,
Is there a good method to hand solder 0402 cap to hard gold plated pads
(30-50 micro inches) and maintain reliability?
It is a design issue. Customer needs to install a BGA socket on top side. So
they specify hard gold plate on BGA area.
But there are lots of caps on bottom side of the BGA and those pads are
plated with hard gold too. No one wants to
scrap those fabs due to hot schedule and high cost. Please advise.
Thanks,
Wei Wang
Process Engineer
Sanmina-SCI
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|