There are several patents on tin-silver-copper alloys. These (in
certain formulations) are patented in Japan (i.e., by Senju) and
elsewhere (i.e., Ames Lab in the U.S.). To promote a patented alloy a
company must have an agreement with the patent holder.
Regards,
David Suraski
AIM
+1-401-463-5605 ext. 5210
www.aimsolder.com
-----Original Message-----
From: Nimal Liyanage [mailto:[log in to unmask]]
Sent: Thursday, September 09, 2004 11:47 PM
To: [log in to unmask]
Subject: [TN] Lead Free Alloy patents
At the first lead free solder conference in MN we all learned that there
are many patents issued to the tin/silver/copper and other lead free
alloys.
Can any vendor manufacture the Japanese adopted alloy
96.5Sn/3.0Ag/0.5Cu and the NEMI alloy 95.5/3.9/0.6Cu for commercial
purposes? As an independent entity, NEMI has conducted extensive studies
on tin/Ag/Cu and I was under the impression that any commercial company
could freely market both of these alloys. Apparently, the SAC alloy
promoted in Japan does not have any patent either.
Any comments?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|