TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Mon, 13 Sep 2004 10:11:47 +0200
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Guenter Grossmann <[log in to unmask]>
Subject:
From:
Guenter Grossmann <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (38 lines)
Carrie

Many voids are caused by poor through hole quality. The reasons are:
- Drills used too long
- Too high feeding rate in the drilling process
- Plating too thin

The voids are not caused necessarily by moisture but by outgassing of
the epoxy and plating residues penetrating along the glass fibres if the
holes are rather ripped than drilled.

I sent a figure from an old survey to Steve to put it on his homepage.
I called it Voids in Solder Joints.

Best regards

EMPA
Swiss Federal Laboratories  for Materials Testing and Research
Centre for Reliability
Guenter Grossmann,  Senior Engineer

8600 Duebendorf
Switzerland

Phone: xx41 1 823 4279
Fax :     xx41 1 823 4054
mail:     [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2