I'm interested in what the "Grand Wazoo" Doug Pauls and Brian Ellis have to say about this. If I've read their musings correctly alcohol does a nice job of spreading the ionic schmootz where DI water cleans it very well.
If my research is correct, there are several automated DI water stencil cleaning systems readily available on the market (www.aqueoustech.com www.aat-corp.com to name just two) and these suppliers also make batch style board cleaners. Austin American (aat-corp) has a new unit on the market for under $10k.
Oops, was that too close to a sales pitch?
Why would you want to "eliminate DI water"?
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Black, Paul
Sent: Wednesday, September 01, 2004 10:58 AM
To: [log in to unmask]
Subject: [TN] Cleaning populated boards with Isopropyl
Hi Everyone,
I currently clean SMT stencils in a sink with hot deionized water. I would like to automate this process (and eliminate the DI water) and have been looking at cleaners that can do the job. One of them uses Isopropyl Alcohol with no rinsing. This should work fine for the stencils but occasionally I also have to clean misprinted boards that may already be populated on one side, using no-clean solder paste. If I were to use this Isopropyl process on the misprints, would I be risking reliability of the board?
Any help would be appreciated.
Thank you,
Paul Black
Manufacturing Engineer
Kronos
E-mail: [log in to unmask]
Voice: (978) 947-1520
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|