Brian,
Foresite Labs (formally CSL) has a real time PowerPoint slide show done
in real time showing a dendrite growing in 12 seconds across a .020 inch
gap at ten volts with a drop of DI water applied (no solder - bare copper).
Quite impressive!
David a. Douthit
Manager
LoCan LLC
Brian Ellis wrote:
> Yes, the film was shot in real time. I believe that it was shot with a
> 10 V DC source via a 10 kilohm current-limiting resistor across two
> adjacent tracks spaced about 1 mm with a single drop of 18 megohm water
> applied. However, I no longer have the details, so may be slightly off
> on some of them. I know that Charles Jennings tried it with different
> substrates and different conductor finishes and succeeded in growing
> dendrites with all of them, though at very different speeds.
>
> Brian
>
> Carl VanWormer wrote:
>
>> Was this growth "real time". If not, how long did the process take?
>>
>>
>> Carl Van Wormer
>> Cipher Systems
>> 1815 NW 169th Place, Suite 5010
>> Beaverton, OR 97006
>> Phone (503)-617-7447 Fax (503)-617-6550
>>
>>
>>
>> -----Original Message-----
>> From: Brian Ellis [mailto:[log in to unmask]]
>> Sent: Sunday, August 29, 2004 12:18 AM
>> To: [log in to unmask]
>> Subject: Re: [TN] Historical Document (Dendrites)
>>
>>
>> Steve
>>
>> As far as I'm aware, this clip is in the public domain. I know that
>> Charles
>> Jennings distributed many 16 mm copies of it. If this is so, then you
>> don't
>> need my permission. If it is considered copyright, then you should obtain
>> permission from Sandia (I don't imagine this would be a problem).
>>
>> Of course, the tiny image in my download is hardly suitable for
>> reproduction. I could provide it in a form reproducible on a TV or
>> computer
>> screen as an SVCD (PAL 480 x 576 pixels 25 fps or NTSC 480 x 480
>> 29.97 fps)
>> or even a DVD (PAL 720 x 576 25 fps or NTSC 720 x 480 29.97 fps). I'd be
>> willing to do this on a non-profit basis, but my costs (media, conversion
>> and authoring time on specialised equipment, packing and postage)
>> would have
>> to be covered. (As I'm "retired", living on a pension, I no longer have a
>> company to sponsor me.) I hope this is not contravening IPC rules on
>> spamming on the TN.
>>
>> Brian
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or
>> 847-509-9700 ext.5315
>> -----------------------------------------------------
>>
>>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|