TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 26 Aug 2004 18:23:38 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (134 lines)
Hi! Depending on which 003A test method you chose either and/or both an
assembly or fabrication house can run the 003A tests. My suggestion would
be to run the Test method S  - surface mount simulation test. A unpopulated
pwb is run through the standard reflow process (stencil paste and then
through the reflow oven) and then inspected for 95% minimum wetting on the
pads. If you have a pwb wetting problem Test S typically can catch it -
especially since Test S uses production materials and equipment. Good Luck.

Dave



                      Ken Patel
                      <[log in to unmask]        To:       [log in to unmask], [log in to unmask], Ken Patel <[log in to unmask]>
                      om>                      cc:       [log in to unmask]
                                               Subject:  RE: [TN] Solderability Issue on ENIG board
                      08/26/2004 06:19
                      PM






No. Who can run it? Can I ask my fab house or assembly house to run it?

Re,
Ken Patel

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, August 26, 2004 4:17 PM
To: [log in to unmask]; [log in to unmask]
Cc: [log in to unmask]
Subject: Re: [TN] Solderability Issue on ENIG board

Hi Ken! Have you run a JSTD-003A solderability test on the suspect pwbs
yet?

Dave Hillman
Rockwell Collins
[log in to unmask]




                      Ken Patel

                      <[log in to unmask]        To:       [log in to unmask]

                      OM>                      cc:

                      Sent by: TechNet         Subject:  [TN] Solderability
Issue on ENIG board
                      <[log in to unmask]>





                      08/26/2004 02:40

                      PM

                      Please respond to

                      TechNet E-Mail

                      Forum; Please

                      respond to Ken

                      Patel









All,
I am finding non-wetting at the certain locations on the boards (four
places
to be exact) where solder is creating golden islands (bec' of ENIG) which
you can see in the picture. In the picture, you can see that toe of pads
does not allow any wetting of the solder.

I would like to get an expert opinion on the subject as why certain
locations have problems and what are the possible reasons for non-wetting.
I
very much doubt this as an assembly problem as peak temp was around 218c
and
solder remains liquidous for more than 45 seconds.



Picture can be found at...Thanks to Daan.

http://www.smtinfo.net/forum/index.php?showtopic=54
<http://www.smtinfo.net/forum/index.php?showtopic=54>



Re,

Ken Patel


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2