Colin:
Here's the link
http://www.datacircuits.com/docs/Material%20Sheet.pdf
Sona Sitapara
----- Original Message -----
From: "Colin Weber" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Sunday, August 22, 2004 6:53 PM
Subject: Re: [TN] Search for HF Laminate Material
> Hi Phil,
>
> I tried that link at the time and it didn't work so I trashed it. Maybe
> there was
> a problem with our Intranet at the time. Do you still have that link?
>
> Tim and Ingemar,
>
> We are not using embedded/buried capacitors. The capacitance we wish to
> achieve is
> on external layers using copper pads. We succeed with the rogers non-UL
> material.
> Now we need to replicate the results with a UL material. We are looking to
> create
> a capacitance of 0.25pF and these are used in sampling 3.5kV of RF. We do
not
> know precisely what didn't work with the UL Rogers material and why the
non-UL
> did work. At this stage we are just trying different materials and looking
> at end results for our application, of which I am unable to describe in
detail.
>
>
> Colin
>
>
> At 01:44 AM 8/21/2004, you wrote:
> >hi,
> >
> >a couple days ago a url was provided that presented a very extensive
table of
> >properties for several vendors laminate products. did you check there?
> >
> >phil
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|