As part of the 4553 I Ag document, we ran I Ag as a surface finish for
Membrane switch applications to 1 million cycles over approximately six
months with NO failures. The 4553 recommends the use of I Ag for membrane
switches for class 1 and class 2 but NOT class 3 applications.
Gerard O'Brien
Photocircuits Corporation
Co chairman 4-14 plating committee.
-----Original Message-----
From: Cal Driscoll [mailto:[log in to unmask]]
Sent: Monday, August 16, 2004 7:20 AM
To: [log in to unmask]
Subject: [TN] silver migration in membrane switches
Hello all-
I am looking for supportive documentation on Silver migration as it pertains
to membrane switches.
Any support on this would be greatly appreciated.
Unfortunately, I do not have any additional information. This was just a
request from my engineering group with no details.
Thanks,
Cal
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|