The trace spacing is violated either by etching, contaminates or
possible voiding the dielectric that insulates the tracks. If the
breakdown involves nets that are connected to utilities, the issue could
be CAF if operating for sometime, or a registration issue with a TH pin
to the plane layer. X-Ray and microsection could provide some useful
information along the affected net and failed areas if indicated by
damage. The 9 KV DWV you state only applies from layer to layer - the
inter-net spacings can be violated any where along the signal run or
utility.
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302-1890
Tel. 802.257.4571.21 Fax. 802.257.0011
[log in to unmask]
http://www.vtcircuits.com
Bill Higinbotham wrote:
>We are using a multilayer FR4 board with 12 mils between layers and
>getting breakdown between traces on different layers. The voltage is
>about 3500 V peak. THis board should be good for 740 V/mil x 12 or 9
>KV. I wonder if it is excessive leakage due to moisture absorption?
>
>Bill
>
>Bill Higinbotham
>RFL Electronics Inc.
>E-mail : [log in to unmask]
>Voice: 973.334.3100 Ext. 386
>Fax: 973.334.3863
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|