TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Baski Devre <[log in to unmask]>
Date:
Thu, 19 Aug 2004 07:24:14 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (53 lines)
Brightner System (airless, RPP, etc), ASF, Anode Ratio and racking system.  Disparties on circuit/panel gemoetry will also create current density differnences from hole center to panel surface. 



Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: Baski Devre [mailto:[log in to unmask]] 
Sent: Thursday, August 19, 2004 1:15 AM
To: [log in to unmask]
Subject: [TN] thickness contol


Dear Technetters,
What are the most effective common factors  of the thickness  contol at the Double Side, Panel plating, PTH process?

Thanks...

Mustafa YÜCEL
Ürün Kalite Mühendisi
Product Quality Engineer

BASKI DEVRE SAN. ve TIC. LTD. STI.
Ceyhan Sk. No:10 81490 Pendik-Istanbul-Turkey
Tel:    00 90 216 3901036 (4 Hat/Line)
      00 90 216 4836560 (4 Hat/Line)
Fax:    00 90 216 3544941
      00 90 216 4913269
Internet:www.baskidevre.com.tr

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2