Joe,
what is the RH on the floor? Thanks.
jk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Macko, Joe @ IEC
Sent: Wednesday, August 18, 2004 1:11 PM
To: [log in to unmask]
Subject: Re: [TN] Polyimide Boards, Aqueous Wash & Baking
Hello,
We just successfully built x number of double sided, rigid-flex polyimide
boards and bake for 4 hrs at 125 C just prior to reflow. Limited floor life
between bake out / reflows to 2 hours, which basically required another bake
out prior to 2nd side reflow.
joe
-----Original Message-----
From: Mike McMonagle [mailto:[log in to unmask]]
Sent: Wednesday, August 18, 2004 9:25 AM
To: [log in to unmask]
Subject: [TN] Polyimide Boards, Aqueous Wash & Baking
I'd like some feedback from folks doing hi-rel assembly with polyimide
fabs. If you perform aqueous wash after during or after soldering
operations, do you perform a post-wash bakeout of the assembly prior to
additional soldering operations? If so, for how long and at what
temperature? I'm trying to correlate a customer specification to good
industry practices, TIA for the inputs....
Mike
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|