Possibly - see http://www.uksteel.org.uk/nw20.htm which puts typical
level of lead in steel used in certain auto steels at .25%.
Regards,
Chris
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Mike Haff
Sent: 23 August 2004 16:45
To: [log in to unmask]
Subject: [LF] Lead free connectors
It was recently brought to my attention (rumored) that connector
manufacturers are not able to meet the 0.1% lead content for standard
I/O
connectors because they have to use high lead content steel in the
forming
of the connector shells in industry standard I/O connectors such as
ubiquitous D-subs, MDR's etc.
Does this ring true? If so does anyone have knowledge of how the
connector
manufacturers are planning on getting around this?
Thanks,
Mike Haff
Enhance, Inc.
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
-------
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose. If you are not
the intended recipient, delete this message. If you are not the intended
recipient, disclosing, copying, distributing, or taking any action based on
this message is strictly prohibited.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|
|
|