Hi Helena,
You certainly have a good idea in mind. In addition to Glenn's comments, may I suggest a checklist of item to specify found in IPC-D-325 under the section 6.0, Master Drawing Notes and Check List. And just an idea: instead of just a couple of templates for your engineers, you could also list all company-accepted variations, processes, etc., in this document, and they in turn could "check off" the ones that their particular project requires. Glenn mentioned 17 surface finishes; your firm may only want to use 3 or 4 of those, and say which is the most preferred (for example):
xx. Surface Finish:
____ A. HASL (please note that this finish is being phased out due to WEEE and RoHS requirements)
____ B. ENIG .000004 immersion Au over .000100 electroplated Ni
____ C. OSP Organic Surface Preservative (preferred) .....
etc., etc.
Best Regards,
Roger
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pasquito, Helena
Sent: Thursday, August 26, 2004 5:45 AM
To: [log in to unmask]
Subject: [TN] Board Fabrication Template
Hello,
We are in the process of standardizing our supplier board fabrication
requirements. We would like to come up with a couple of boiler plate type
templates for our design engineers to use. Do any of you have such a
template that you could share or know where I can find one? It would be
highly appreciated so that we do not have to re-invent the wheel.
Regards,
Helena
Helena Pasquito
Mfg. Skills Training Instructor
Customer Relationship Management
Tyco Electronics M/A-COM
1011 Pawtucket Blvd. M/S150
Lowell, MA 01853
Phone 978-442-5024
Email [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|