Cheryl,
Many have suggested using a balance, but if you go this way, you need to
have a set time after putting it on the scale before you take a reading.
The weights are constantly changing in the 3rd and 4th decimal place,
especially with low solids fluxes that have a high level of isopropanol
carrier. You also need to have a method of keeping the flux from dripping
onto the pan or into the scale itself.
Doug Pauls
Cheryl Tulkoff
<cheryl.tulkoff@N To: [log in to unmask]
I.COM> cc:
Sent by: TechNet Subject: [TN] Tool for measuring amount of flux applied
<[log in to unmask]>
08/18/2004 08:26
AM
Please respond to
TechNet E-Mail
Forum; Please
respond to Cheryl
Tulkoff
Can anyone recommend an accurate tool or method for measuring the amount
of liquid flux applied by a spray fluxer for the wave solder process?
Thanks!
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------