Speaking from experience, merely calling out a higher Tg for lead-free
can may cause you some pain. You also need to be sure that the Td
(thermal decomposition point) is elevated above your maximum process
temperature. If not, you may be susceptible to measling/delaimination.
One way to insure this is be sure that the laminate is not DICY cured.
Check out some of the technical papers at www.isola-usa.com.
Rich / KEDS
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Klawson
Sent: Monday, August 16, 2004 8:03 AM
To: [log in to unmask]
Subject: [TN] Laminate Tg specifications
What is the best way to specify laminate glass transition temp
(Tg)? These are the types of products we deal with, any
recommendations
on what Tg's we should call out? Call them all150C minimum and be done
with it? And what about lead-free processes with higher reflow temps,
do we need higher Tg's?
1.) Standard through-hole 6 to 10 layer wave solder single pass, assume
2x rework
2.) Standard SM 8 to 16 layer, 2x SM reflow, 1x wave solder palletized,
2x rework
3.) Complex SM 12 to 24 layers, 2x SM reflow, 1x wave or selective
solder, 2x rework
Thanks in advance for your wisdom.
-- Gregg
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|