Virtually any sort of pre-finishing you do to high Silicon Aluminum creates problems, as Al is so readily attacked by almost any cleaner, at either end of the pH scale, and the Silicon is not, so the Silicon forms a loose, but extremely difficult to remove, smut.
We offer a desmut for Aluminum specifically formulated to address this issue... the difference in the parts when using normal Al desmuts, vs this product is slightly amazing.
I suspect that the plating on high Si parts, treated with a typical desmut will have serious adhesion problems.
Rudy Sedlak
RD Chemical Company
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
Yahoo! Mail - 50x more storage than other providers!
|
|
|