Silver sulfides readily and copper somewhat less so in the presence of
sulfur (atmospheric hydrogen sulfide and sulfur dioxide gases). This is
normal. The immersion silver is thin and sufficiently porous for the
underlying copper also to be sulfided. Stopping atmospheric pollution
from fossil fuels would go a long way towards slowing down the problem,
although there are other sources of sulfur gases (including eggs!)
Brian
David Yeh wrote:
> Hi,
>
> Can anyone share experience relating to tarnish immersion silver on the test vias area? The observation is there is blackish substance that seems to bloom (blossom) out of the test vias. The EDX analysis seems to show Ag , S and Cu on the blackish substance.
>
> Would appreciate information of phenomenon mechanism and causes. Many thanks.
>
> David.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|