TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Ken Patel <[log in to unmask]>
Date:
Thu, 26 Aug 2004 12:40:49 -0700
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Patel <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
All,
I am finding non-wetting at the certain locations on the boards (four places
to be exact) where solder is creating golden islands (bec' of ENIG) which
you can see in the picture. In the picture, you can see that toe of pads
does not allow any wetting of the solder.

I would like to get an expert opinion on the subject as why certain
locations have problems and what are the possible reasons for non-wetting. I
very much doubt this as an assembly problem as peak temp was around 218c and
solder remains liquidous for more than 45 seconds.



Picture can be found at...Thanks to Daan.

http://www.smtinfo.net/forum/index.php?showtopic=54
<http://www.smtinfo.net/forum/index.php?showtopic=54>



Re,

Ken Patel


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2