TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Wed, 18 Aug 2004 05:18:07 -0700
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Blair K. Hogg" <[log in to unmask]>
Subject:
From:
"Blair K. Hogg" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (261 lines)
Does it have the solutions to the problems too?

>>> [log in to unmask] 08/18/04 08:14AM >>>
1st:May I point out that the fishbone diagram is not my creation.
2nd: As so many want it (surprise! Do professionals like you need such crib?), maybe Steve can put a copy on his homestead. Watt do u zink, Steve?

Ingemar

PS. fishbones are excellent for teaching the mysteries of SMT, you get a knowledge platform, but they don't automatically guide you to the root of a specific Murphy day problem.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Marvin Gaines
Sent: den 18 augusti 2004 13:49
To: [log in to unmask] 
Subject: Re: [TN] Most common PCB failure modes


Kristopher,

My experience in this matter is that PCB manufacturing companies
have not had one common defect that can be detailed as a persistent problem
unless they
have a process issue and then the defect should be able to be traced to a
date code).
Usually there is a myriad of issue's that the public never knows about.
As with all manufacturing there are issue's that come up and make it
ultimately to the end customer.
So to pinpoint one common problem would be difficult.


Ted Gaines
Ht&D Cam Service
775-599-6720

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Naisbitt
Sent: Wednesday, August 18, 2004 7:11 AM
To: [log in to unmask] 
Subject: Re: [TN] Most common PCB failure modes


Hi Kristopher

All our customers tell us they have zero defects and no failures.

We call this "Telling Porky Pies".

I did a net search on your question and came up with one that might be
useful: http://www.allaboutcircuits.com/vol_5/chpt_8/5.html 

--
Regards Graham Naisbitt

[log in to unmask] 

Concoat Limited - Engineering Reliability in Electronics
A British Manufacturer

www.conformalcoating.com      www.concoat.co.uk     www.concoatsystems.com 

Golf Quote of the week: If you think its hard to meet new people, try
picking up the wrong golf ball.

Cell: 079 6858 2121
Office: +44 (0)1252 813706



> Hello,
> Could some of you share what are the most common PCB defects that escape
to
> your customers?
>
>
> Thanks
>
> Kristopher J. Keating
> Circuit-Wise, Inc.
> 400 Sackett Point Rd.
> North Haven, CT 06473
> tel. (203) 281-6511 x 410
> fax (203) 287-8409
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
> (KC/EMW)
> Sent: Tuesday, August 17, 2004 3:16 AM
> To: [log in to unmask] 
> Subject: Re: [TN] thin film
>
> Seal Science say they have it all:
> http://www.sealscience.com/html/products/VacuumCupsPdfs/15about.pdf 
> ultrahighvacuum guys use pure gold gaskets:
> http://www.sisweb.com/catalog/F39.pdf 
> ourselves, we use as simple as butyl rubber:
> http://www.allstategasket.com/materials.asp (not Ultravacuum, of course)
> Butyl rubber group includes ordinary rubber used in your mountainbike
tire,
> can keep vacuum or pressure for very long time.
> /Ingemar
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Crepeau, Phil
> Sent: den 17 augusti 2004 02:25
> To: [log in to unmask] 
> Subject: Re: [TN] thin film
>
>
> hi,
>
> i believe you should be able to use a gasket material such as viton.
>
> phil
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Douglas O. Pauls
> Sent: Monday, August 16, 2004 2:02 PM
> To: [log in to unmask] 
> Subject: [TN] thin film
>
>
> Good day all,
> I am in need of a recommendation for a thin film sealant material.  I need
> it to be 15-20 mils thick, cuttable, and preferrably non silicone.  We
have
> considered the Sil-Pad technology, but as this will be used in a vacuum
seal
> operation, I am concerned about silicone outgassing or cross
contamination.
> Are there any thin gasket materials from the engineered rubbers that
anyone
> would recommend?
>
> Doug Pauls
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> --
> Incoming mail is certified Virus Free.
> Checked by AVG Anti-Virus (http://www.grisoft.com).
> Version: 7.0.262 / Virus Database: 264.6.1 - Release Date: 8/16/2004
>
>
> --
> Outgoing mail is certified Virus Free.
> Checked by AVG Anti-Virus (http://www.grisoft.com).
> Version: 7.0.262 / Virus Database: 264.6.3 - Release Date: 8/16/2004
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3..16 
for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.

This footnote also confirms that this email message has been swept
for the presence of computer viruses.

www.hubbell.com - Hubbell Incorporated

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2