Hey all,
I have a minor problem with a component in house. The component leads
are 19 AWG nickel and I need to connect to them using 20AWG copper wire.
I looked in the archives for previous discussions on this topics and
came away with the impression that OA flux is required. My question is:
Can I solder these parts without having to go out and get some OA flux?
We use RMA and I'm reluctant to bring in a different flux and have it
used rather than the RMA. Can one mechanically prep the leads, then
flux with RMA, then dunk in the solder pot?
Thanks in advance for all your input!
Eric Kalgren
Manufacturing Engineer
Atlantic Microwave
Phone: 978-779-7062
Fax: 978-779-0101
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------