Sure - I will forward to you some robust builds for 4-20 layer circuits
later today.
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302-1890
Tel. 802.257.4571.21 Fax. 802.257.0011
[log in to unmask]
http://www.vtcircuits.com
-----Original Message-----
From: Tempea, Ioan [mailto:[log in to unmask]]
Sent: Tuesday, July 13, 2004 10:32 AM
To: [log in to unmask]
Subject: Re: [TN] Board Stack geometry
Jeffrey,
could you write down for us an example of good stackup specification?
Something that gives enough freedom to the fab, so that they do a
competitive quote, but also keeps a rigorous functional spec, that is
portable when the board supplier changes.
Thanks,
Ioan
> -----Original Message-----
> From: Jeffrey Bush [SMTP:[log in to unmask]]
> Sent: Tuesday, July 13, 2004 10:15 AM
> To: [log in to unmask]
> Subject: Re: [TN] Board Stack geometry
>
> If needed for performance, the stackup on the drawing should only
> specify the required dielectric thickness and finished copper weights.
> The PCB can be constructed in many several methods to obtain the
> desired end thickness. If, for example, you spec out some plies of
> 2116 glass in an opening, and supplier B only uses 2165, this becomes
> an issue. If signal/performance integrity is not an issue in the
> design, leave it up to the PCB fab house and the compliance testing to
> your drawing requirement to ensure thermal and mechanical integrity is
> there.
>
>
>
> Jeffrey Bush
> Director, Quality Assurance and Technical Support
>
> 76 Technology Drive - POB 1890
> Brattleboro, Vermont 05302-1890
> Tel. 802.257.4571.21 Fax. 802.257.0011
> [log in to unmask]
> http://www.vtcircuits.com
>
>
>
> -----Original Message-----
> From: Roger Stoops [mailto:[log in to unmask]]
> Sent: Tuesday, July 13, 2004 9:05 AM
> To: [log in to unmask]
> Subject: [TN] Board Stack geometry
>
>
> This brings up a question I have had bumping around in my head for a
> while, for example:
>
> A pcb has been designed, assembled, tested, and now goes through FCC
> and CE emissions and susceptibility testing. The board stack was
> determined by the pcb vendor. The assembly passes first time.
> Purchasing or the EMS finds a less expensive yet reliable board house
> and buys production boards from this new house. The new house changes
> the board stack to their preferred lay-up.
>
> Would not this board need re-testing for FCC/CE
> emissions/susceptibility? For boards requiring this type of testing,
> would not a board stack specified on the print be required?
>
> TIA and much appreciated,
>
> Roger Stoops
>
>
> -----Original Message-----
> From: Jeffrey Bush [mailto:[log in to unmask]]
> Sent: Monday, July 12, 2004 8:40 AM
> Subject: Re: 7628 prepreg?
>
>
> Common type, stable, low resin content and likely predicable thickness
> is this is important. Otherwise PCB house should be left to determine
> the optimal stack for the board geometry and end use.
>
>
>
> Jeffrey Bush
> Director, Quality Assurance and Technical Support
>
> 76 Technology Drive - POB 1890
> Brattleboro, Vermont 05302-1890
> Tel. 802.257.4571.21 Fax. 802.257.0011
> [log in to unmask]
> http://www.vtcircuits.com
>
>
>
> -----Original Message-----
> From: Brooks,Bill [mailto:[log in to unmask]]
> Sent: Friday, July 09, 2004 5:08 PM
> To: [log in to unmask]
> Subject: [TN] 7628 prepreg?
>
>
> Bill Brooks
> PCB Design Engineer , C.I.D., C.I.I.
> Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 http://pcbwizards.com
>
> Why would a designer specify 7628 prepreg in the construction of a
> board? What characteristics are unique to it? Bill Brooks, CID
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|