What we see coming in, and suggest to our customers making this transition
is to simply state what you wrote.
Finish: Immersion Tin
or
Finish: OSP
We take care of the rest...
As for thickness requirements, well you really can't under or over plate
these two finishes very easy...
Franklin
----- Original Message -----
From: "Kane, Joseph E" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, July 01, 2004 4:04 PM
Subject: [TN] Specifying PWB Finishes
> We're preparing to order some test boards with alternative finishes for
> lead-free
> testing, including immersion tin and OSP over bare copper. Can anyone
> suggest
> how we might specify these board finishes in a drawing note? Our existing
> drawings pretty much specify only the material and the thickness,
something
> like "immersion gold, xxx thick, over electroless nickel, xxx thick."
>
> Joe Kane
> BAE SYSTEMS Controls
> Johnson City, NY
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|