You must need your DPMO (Defects Per Millions Opportunities) per each
process and Yield for each product.
The cost of the repair of each defect (SMT, TH, BGA, Press fit etc.) should
be quantified
When you have the data, you can calculate the repair costs otherwise you
can .
--------------------------------------------------------------------------------------------------------------------------
Best Regards
Reuven ROKAH
e mail: [log in to unmask]
Suzanne Foulkes
<[log in to unmask] To: [log in to unmask]
COM> cc:
Sent by: TechNet Subject: [TN] Rework Costs
<[log in to unmask]
>
28/07/2004 14:29
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to Suzanne
Foulkes
I was asked the question if I could quantify results in a dollar amount
for the defects and rework we are doing in our manufacturing process.
I'd like to know how other people put a cost to rework. All suggestions
appreciated
Sue Foulkes
QA Manager
Akron, Ohio
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|