Siggi: I'm not sure why you can't use a 2 component glue. "long stick time"
are you saying that the cure time is too long? If that's the case there are
many fast set, 2 part epoxies that will bond very well to a PCB and/or
soldermask substrate. These will cure in less than 5 mins at 23C.
There are some that will cure even faster but the adhesive mass must remain
small to prevent excessive exotherm.

Loctite, CIBA, 3M, etc, all make a variety of these fast curing 2 part epoxy
structural adhesives.

                                                                Regards

Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-446-6076


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Zweigart, Siegmund
Sent: Friday, July 02, 2004 8:29 AM
To: [log in to unmask]
Subject: [TN] Glue on PCB


Hello all

I have to Glue some guidepins to a PCBA. Can anybody give some inputs which
glue is possible?
I think cyano based glues are not possible on soldermask / PCBA.
2 component glue are no option due to long stick time.

Any recommendations?

Best regards

Siggi

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2