TECHNET Archives

July 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Thu, 29 Jul 2004 13:31:30 +1000
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, DUTTON Phil <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
DUTTON Phil <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Thanks Werner and Shean,

This adds to my concern about the missmatch. This is a large device (40mm)
so these issues are fairly important. 
I was worried about the pad pulling all of the solder from the joint and creating an open, but it seems that even an otherwise good, but assymettric joint can also cause problems.
I can't really do anything about the sphere diameter unfortunately.
I had thought of using SMD pads, but I'm convinced that that will cause a greater problem with the sort of stress concentrating geometry created in the resultant joint. 

regards,

Phil.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Shean Dalton
Sent: Thursday, 29 July 2004 4:34 AM
To: [log in to unmask]
Subject: Re: [TN] BGA pad missmatch


Hi Phil,

I have been hoping for a response from someone who has practical
experience with this, as it is interesting to me.  That said, I suspect
areas of concern would be for TCE.  The larger pad size takes away
solder from the bulk joint, effectively reducing the standoff height.
Again, I suspect the reduced standoff height might reduce the "flexure"
ability of the solder joint to "absorb" the TCE mismatch.    And, using
a larger sphere diameter may compensate for the large pad size,
effectively raising the standoff height.  Sure would be nice to do a
finite elemental analysis.

Have fun!,

Shean Dalton
Austin American Technology
www.aat-corp.com <http://www.aat-corp.com>


-----Original Message-----
From: Werner Engelmaier
Sent: 7/28/2004 1:46 PM
To: [log in to unmask]
Subject: Re: [TN] BGA pad missmatch


Hi Phil,
Land area is not the issue, solder joint geometry is. If the unequal
soldering areas create solder joint geometries with stress
concentrations, earlier
failures [everyting else can be anticipated]. This is similar to NSMD
vs. SMD
solder pads.

Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2