Land patterns don't need to change - but the apertures on the stencil may
need enlarging. Typically, LF paste doesn't wet as well as Pb pastes.
Regards,
Danielle
Danielle L. Casha
Process Technician
EPM
Tel: 905-479-6203 ext. 272
Fax: 905-479-6990
Website: www.epmnet.com
-----Original Message-----
From: Pratap Singh [SMTP:[log in to unmask]]
Sent: Wednesday, July 21, 2004 3:14 PM
To: [log in to unmask]
Subject: Re: [LF] LeadFree and Land Patterns
Roger,
No need to fret. Land pattern should not be affected by converting to LF
solder. Depending upon the solder used, reflow profile settings will
change since LF solders flow at higher temperature.. Visual inspection
and void inspection should also remain same.
_____________________
pratap singh
Tel./Fax: (512) 255-6820
email: [log in to unmask]
www.rampinc.com
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET
Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|
|
|