I presume then that Nortel will NOT be taking an exemption under the ROHS
annex covering internet infrastructure??..........................or are you
on a more philosophical discussion?/
John
-----Original Message-----
From: Pascal Guiheneuf [mailto:[log in to unmask]]
Sent: Friday, July 02, 2004 11:45 AM
To: '(Leadfree Electronics Assembly Forum)'; 'John Burke'
Subject: RE: [LF] tin pest
In france we have a popular expression "avoir du plomb dans la tete", maybe
translated by "having lead in head". Coming from the "lead poisoning"
disease, it describes somebody stupid. Lead is hazardous, and especially for
children. It attacks the brain.
In 1973, lead was banned from gazoline, in 1978 from paints, beginning of
XXI century from all water pipes (they have to be changed before 2010 or
something like that in Europe), now it is time for electronics.
Lead has to be removed, and solutions to issues will be found by people with
functioning brain.
Cordially,
Pascal
-----Original Message-----
From: John Burke [ mailto:[log in to unmask]
<mailto:[log in to unmask]> ]
Sent: vendredi 2 juillet 2004 19:04
To: [log in to unmask]
Subject: Re: [LF] tin pest
Wouldn't that be a story:
"A team of Antarctic researchers investigating effects of electronics
manufacturing on the ozone layer were stranded today when their GPS system
malfunctioned. The malfunction is thought to be associated with the removal
of lead from the solder"..................8-)
John
-----Original Message-----
From: MA/NY DDave [ mailto:[log in to unmask] <mailto:[log in to unmask]> ]
Sent: Friday, July 02, 2004 9:37 AM
To: [log in to unmask]
Subject: Re: [LF] tin pest
Hi Jim, Tyco-Bob, Jean-Paul, and IPC LF Listservers,
<Thank you for your response. Like many other issues in this Lead-Free
transition, it sounds as if "tin pest" has been overblown.>
I am not sure YET that the issue is overblown. I believe that based on the
environments of certain products or certain product life conditions that we
may see this selectively in real life applications. In June Tin's KayN
(Soldertec) did respond to us that ITRI has not seen any effect and
privately others have also written to me that they have yet to see any
effect.
My first guess is product that has to survive continual cold temperatures
like in the Artic or in refrigerator/freezers where -40C/-40F is common or
in other applications like thermoelectric coolers.
As for a nucleation site for the transformation to get started, I am less
clear of how that all happens. More Study, or the Luck of being an IPC LF
Listserver is needed.
If you look at the UK's Open University Report it seems obvious that we will
see this under certain conditions. The sample just had too too much Tin Pest
to be a coincidence.
Yours in Engineering, Dave
Y i Engr, MA/NY DDave
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Leadfree To temporarily stop delivery
of Leadree for vacation breaks send: SET Leadfree NOMAIL Search previous
postings at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
---
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Leadfree To temporarily stop delivery
of Leadree for vacation breaks send: SET Leadfree NOMAIL Search previous
postings at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|