Look up "vapor pressure". The vapor pressure is not zero even far below the
boiling point.
> -----Original Message-----
> From: Leadfree [mailto:[log in to unmask]] On Behalf Of Harvey Miller
> Sent: Tuesday, July 13, 2004 12:12 PM
> To: [log in to unmask]
> Subject: [LF] "lead vapors" myth
>
>
> Recently Pascal from Alcatel, Ted Smith of Silicon Valley
> Toxics Coalition, among others, have refer to lead vapor
> exposure to Chinese recyclers dismantling populated PC
> boards. Most participants know that this is a fiction; the
> "vapors" are flux, not healthy, but not lead. But I thought
> I'd check the actual parameters
>
> Handbook of Chemistry and Physics says that lead boiling
> temperature is 1780 degrees C. Trade sources say that
> soldering irons attain 300 degrees C.
>
> The lead vapor myth should be nailed.
>
> --------------------------------------------------------------
> -----------------Leadfee Mail List provided as a service by
> IPC using LISTSERV 1.8d To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Leadfree To temporarily stop delivery
> of Leadree for vacation breaks send: SET Leadfree NOMAIL
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> --------------------------------------------------------------
> -----------------
>
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|
|
|