Jim
What you're describing is also called double reflow. It has been discussed on Technet. Suggest you search the archives. George Wegner has significant experience with this also.
The failure mechanism occurs when previously soldered surface mount components are exposed to "almost" reflow temperatures. Based on the thermal source (frequently a secondary wave solder operation) the primary components approach reflow temperature. As the temperature increases, the strength of the solder connection decreases. Thermal mismatch between the component and substrate result in stresses. In some cases, there is sufficient stress to initiate a crack in the intermetallic region between the pad and the solder joint. The crack propagates through the intermetallic boundary until the joint fails. The result is an open and possibly a part that falls off of the board. It's really strange to see a gull wing device that came off of the board and the solder joints are undisturbed to an extent that one could believe that the board and copper pad were somehow dissolved.
As I said initially, check previous postings for more details.
Don Vischulis
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Marsico, James
Sent: Tuesday, July 20, 2004 2:29 PM
To: [log in to unmask]
Subject: [TN] PWB SOLDERABILITY
Good Day Technet:
Here's an unusual situation. We recently got a lot of PWBs from our
supplier who we've been using for years. The solder on the boards (HASL)
looks good, thick and shiny. A couple of weeks ago, after SMT assembly with
a fairly aggressive water soluble solder paste, we noticed that one of the
components (diode) had fallen off and was sitting on the operator's bench.
The pads on the board where the component had fallen off showed bare copper,
while the solder fillets remained on the component! Thinking that this was
an unexplainable one-time occurrence, the component was soldered back on and
the board went on its merry way. Well, a couple of days later, boards from
the same lot were soldered and we noticed that some of unused pads or test
pads were copper only, with no traces of solder. We then took some bare
boards, all of which looked good, and ran them trough our reflow and in-line
cleaning process (no flux or solder paste). Low and behold, on about 20%
of the boards there were copper pads with no solder, and a few pads where
the solder was partially peeling off the pads, exposing the copper
underneath (with no traces of copper on the pealed solder). After
discussions with our supplier, we both came to the conclusion that some of
the boards must have been oxidized to such a degree that solder coated the
pads but did not achieve a metallurgical bond. I would have thought that
such a condition would result in a de-wet or non-wet condition, but, as I
said earlier, the boards looked great!
Has anyone else ever come across this before?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|