Rich,
I don't know if your using a fixture or not but if you are two options
are a angle approach to the wave, or adding a thieving device to the
trailing edge of bridging area. Please feel free to contact me offline
if you want more info.
Chad Haima
Pentagon EMS
503-924-2747
www.pentagon-ems.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rich Lasko
Sent: Thursday, July 22, 2004 10:32 AM
To: [log in to unmask]
Subject: [TN] Solder Bridging on a Thru-hole connector
Hello everyone,
I am currently encountering a wave solder issue that I would like to ask
your opinion about. I have a dual row connector (Molex part #
70246-1621) that accumulates soldering bridging in a group of three. I
sent Steve an e-mail to see if he could post the picture on his website
so hopefully he can but until then I'll try and give you a generic idea
of how it is bridging. (The "arrow's" below represent the bridging
between the leads) The wave operator has tried different speeds and
board directions but continues to struggle with this particular
connector.
If anyone has any input I would appreciate it.
TIA,
Rich
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|