What type of components is this happening around?
-----Original Message-----
From: Lance Mayes [mailto:[log in to unmask]]
Sent: Wednesday, June 09, 2004 6:18 PM
To: [log in to unmask]
Subject: [TN] Conformal Coating
Importance: High
Hello again Techies;
We are having issues with our conformal coating on some of our components.
It pulls back from some of the components leads along the edges.
We are wondering if this will make a difference in the protection of the
board.
We're using Humiseal Acrylic 1B31 and Humiseal Thinner 521 in a mixture.
The conformal machine sprays a nice coating and then the coating starts to
recede. Sometimes this happens even when we paint the acrylic manually.
Has anyone else ran into this problem, and what to do to overcome it?
This is a good one for the end of the day. I'll be waiting.
Thanks again
P. Lance Mayes
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
Mfg. Trainer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|