Chad,
The G10/FR4 type you remember are made by Stevens Products @ 973-672-2140
Their web site is: http://www.stevensproducts.com/cguard.htm
We've used them for years. Many different (off-the-shelf and custom) sizes
for goldfingers, connector protectors, board edge stiffeners.
Al Kreplick
Sr. Mfg. Eng.
Teradyne, Inc.
500 Riverpark Drive
Mail Stop NR500 1-1
North Reading, MA 01864
Tel: 978-370-1726
Fax: 734-661-5352
Pager: 888-561-6485
Chad Haima
<chadh@PENTAGON- To: [log in to unmask]
EMS.COM> cc:
Sent by: TechNet Subject: [TN] Goldfinger Masking
<[log in to unmask]
>
06/08/04 04:15
PM
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to Chad Haima
Technetters,
Anybody know of a good source for goldfinger protection? I seem to
remember
one exhibiting at Apex a few years back. Have a customer that is currently
taping them off and of course is looking for an easier more cost effective
way to mask. If I remember right they were made out of G-10/FR-4 type
material.
Thanks,
Chad Haima
Pentagon EMS
Ph: 503-924-2747
Fx: 503-924-2744
[log in to unmask]
www.pentagon-ems.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|