Hi Steve,
We are getting "dummy" BGA packages with 95.5%Sn/4.0%Ag/0.5%Cu.
I have also seen 96.5%Sn/3.0%Ag/0.5%Cu
We are getting µBGA packages with 96.5%Sn/3.0%Ag/0.5%Cu
Also available is 96.5%Sn/3.5%Cu
I hope this helps!
Sincerely,
Debbie Goodwin
Account Representative
10867 Portal Dr
Los Alamitos, CA 90720
Phone = (714) 252-0010
Fax = (714) 252-0026
[log in to unmask]
PLEASE NOTE - Over 90% of all SMT packages are now available Lead-Free!!!
__________________________________________________
This message is intended for the use of the individual entity to which it is
addressed and may contain information that is privileged, confidential and
exempt from disclosure under applicable law. If the reader of this message
is not the intended recipient, or the employee or agent responsible for
delivering the message to the intended recipient, you are hereby notified
that any dissemination, distribution or copying of this communication is
strictly prohibited. If you have received this communication in error,
please notify us immediately by calling
714.252.0010 or returning the original message to us. Thank You.
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Friday, May 28, 2004 7:30 PM
To: [log in to unmask]
Subject: [TN] Lead Free BGA's...
Hi ya'll!!!
I know most everyone is out for the Memorial day holiday, so this will be
something that
everyone can look at on Tuesday...
My question is; what are the spheres going to be made of for "Lead-Free"
BGA's? What about the BGA's (ceramic ones usually) that have "High-temp"
balls?
The high-temp balls are mostly lead, right?
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|