I know this is going to rub a few people the wrong way and it will for
eberhard for me to be taken seriously again, given my abrasive nature, but
masking my inhibitions I will tell about a process I have used.
Take an electric erasure with a gray number 4 ink erasure in it and using an
erasure shield match the opening in the shield to the area you want to
remove the mask. With technique you can just remove the mask and leave the
area shiny that you want to solder. A little IPA to clean the area, the
right flux of choice and you have a good solder connection.
Logic will dictate your process, but it is very quick and easy. We have went
through Qual test with this.
Dewey
-----Original Message-----
From: Franklin [mailto:[log in to unmask]]
Sent: Wednesday, June 30, 2004 5:25 AM
To: [log in to unmask]
Subject: Re: [TN] Soldermask on PTH pad???
Short of very expensive laser strip processes a razor knive and lots-o-labor
are about the only way...chemicals and other type methods are only messy and
cause other problems...
Franklin
----- Original Message -----
From: "Ken Patel" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, June 29, 2004 6:41 PM
Subject: [TN] Soldermask on PTH pad???
> Technetters,
>
> We have pads of hand soldering locations covered with solder mask making
it
> difficult to solder. Is there any other way to solder besides scarping the
> solder mask (abrasive) and use solder fountain? I am looking for any easy
> way to remove solder mask or soldering technique.
>
>
>
> Any help will be highly appreciated.
>
>
>
> Re,
>
> Ken Patel
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|