Polyclad and Isola websites have all the information you need (even if you
are buying other materials, shhhh)
As for specific temperature ratings, you need to make sure the Tg is suited
for the end use, for example, you might not want to use a material with Tg
of 130 in a hot, humid, hostile type environment, not matter what the cost
savings are...
Franklin
----- Original Message -----
From: "Victor G. Hernandez" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, June 02, 2004 11:22 AM
Subject: [TN] Laminate Rating
Fellow TechNetters;
Where can I get information on Laminate rating such as FR1 versus FR4
application with regards to Tg.
Can these laminate be interchange due to cost? What are the Pros and
Cons with this issue.
In advance I thank you for sharing your experience with me.
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|