No.
Checking viscosity of paste is not that easy and our experience on this is
that we tend to have lots of fruitless dialogue with the small number of
people who still do it as a hang over from times past. The dialogue is
debating the relevance or otherwise of small differences in numbers which
are actually caused by faulty customer technique.
You should be able to locate a ship to line paste supplier so there is no
need to check solder paste on receiving.
In use it is better to control the paste by monitoring rate of issue to
line. This will ensure paste is as near to as received condition as possible
when used. We have an Apps sheet on this on our web site. (Or at least we
should have by now, if not contact me and I will send you the text for it if
you are interested).
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Grant Emandien
Sent: 07 June 2004 11:13
To: [log in to unmask]
Subject: [TN] Paste Viscosity measurement on production
Hi All,
We currently monitor temp/humidity of our SMT environment - would there be
added value by introducing viscosity checks? (we do not experience
viscosity-related defects)
TIA
Gramt
**********************************************************************
Relevant company disclaimers are available at the following addresses:
Tellumat (Pty) Ltd e-mail:
mailto:[log in to unmask]
Syntell (Pty) Ltd e-mail:
mailto:[log in to unmask]
Web: http://www.tellumat.com/email.aspx
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
:::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|