Very small connections will provide sufficient connectivity to pass
electrical continuity testing. I would make sure that the testing
parameters are correct - at least 100VDC, with a threshold of 10 OHM to
10 MEGOHMs for continuity and isolation. One important element in this
is the microsection testing program. Barrel cracking is generally a
ductility issue with the plating deposit, which could be aggravated by
excessive thermal excursions, substandard construction/base laminates.
Implementing a comprehensive microsection analysis program will prevent
this issue from being delivered to the field. This is a current
requirement of both MIL and Commercial standards and you supplier should
be able to provide evidence of this program to you on request.
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302-1890
Tel. 802.257.4571.21 Fax. 802.257.0011
[log in to unmask]
http://www.vtcircuits.com
-----Original Message-----
From: Sherif Refaat [mailto:[log in to unmask]]
Sent: Friday, June 11, 2004 11:20 AM
To: [log in to unmask]
Subject: [TN] Electrical Test capabilities
Importance: High
Hi Technetter,
I've got some questions regarding bare boards Electrical testers
capabilities.
1) Is it correct that bare boards electrical testers may not detect
opens caused by complete copper cracks (circomfrential) inside via holes
because the pressure from the test pins do close the crack? ( I
personally do not think so. The copper crack width measured from the
cross section is 0.0004"). The boards I'm talking about are Immersion
Silver plated.
2) How about via copper cracks if the boards are HASLed. Would the
Tin/lead inside the via holes allow enough conductivity to "hide" the
copper crack?
3) If the copper plating thickness inside the hole is considerably
reduced (for example, down to 0.0004" from 0.001") would that be
detected by the E-tester as high resistance?
4) How the test parameters affect the above issues?
Your response is greatly appreciated.
Have a good weekend.
Sherif Refaat, Eng.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|