A soldering only solution would have to involve the columns of solder being
flexible enough to absorb stresses. Or strong enough not to break under
them.
Stronger alloys are probably out. Better thermal fatigue properties almost
inevitably go with higher melting points. Possibly an SAC alloy as developed
for PB-free would represent the minimum change in alloy here, but then you
would need to look at board and component finishes everywhere else.
So the other possible solder only answer to investigate would be to make the
columns "bendier".
Either by making them taller.
Or by using a more "giving" alloy.
This is a property of In/Pb alloys and there are combinations with similar
melting ranges to Sn/Pb, [or higher/lower]. The difficulty then will be to
selectively apply them (their cost makes it worthwhile spending time on
this). You could for example blank off the chip pad openings and then
stencil, dot dispense as required with In/Pb, p&p and then go to reflow as
now.
Which ever way you go will need some study and thought.
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Timo Culmann
Sent: 04 June 2004 08:42
To: [log in to unmask]
Subject: [TN] Ceramic chips on FR 4 CTE Problem
Hello,
we have following problem:
We are using ceramic chips on FR4 due to the temperature cycles we use
during burn in (-40 to +85°C) the chips are sheared of the board. I know
that there is the possibility to solder column interposers onto the chips.
But doing this we would loose the warranty on the chips which we don't
want. We need a soldering solution between chip and board. Is there a
company that offer mezzanie ype of boards with a material that takes the
CTE? A solution converting the BGA to a PGA is not possible due to
vibration in the application.
Any other solution??
Thanks a lot
Timo
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
:::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|