TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Fri, 25 Jun 2004 12:05:42 -0100
Reply-To:
Subject:
From:
Roger Tingler <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (145 lines)
On the other hand, you can apply a conductive epoxy to the hole. If
processed properly it will finish out
with a very small convex pad to a perfectly flat pad.

Roger Tingler
Methods Engineer
Colonial Circuits Inc.
V:800-578-9602 ext:102
F:800-578-0856
E-mail:[log in to unmask]






-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Vladimir Igoshev
Sent: Friday, June 25, 2004 2:38 PM
To: [log in to unmask]
Subject: Re: [TN] VIA in Pad


Just to add to what Tom has said, voids are usually not huge (if everything
is fine with the process), so it should be nothings to worry about. In
addition, similar voids are not uncommon thing  even in the joints on
microvia-free pads.

Vladimir Igoshev,
Research in Motion
451 Phillip St.
Waterloo, ON, N2L 3X2

Voice: (+1) 519-888-7465, ext. 5283
Fax: (+1) 519-886-0863
E-mail: [log in to unmask]


-----Original Message-----
From: Daan Terstegge [mailto:[log in to unmask]]
Sent: Friday, June 25, 2004 11:29 AM
To: [log in to unmask]
Subject: Re: [TN] VIA in Pad


Hi Tom,

You will get voids in the solderjoints.
This is not necessarily a bad thing, but some would argue it is outside
the limits of the IPC-A-610. If you read it carefully, you will see that
IPC-A-610 gives a lot of freedom with respect to voiding (it suggests
some inpection criteria, that's all), so you have to ask the question if
everyone involved with the acceptance of the products is a carefull
reader.

Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net

>>> [log in to unmask] 06/25/04 05:19pm >>>
We're a CM.  One of our customers is asking us to build a board
assembly
that will be using BGAs with VIAs in pads.  They are in the design
stages at
this point, and we have some concerns with having a Via in the middle
of a
BGA pad.  Anyone have suggestions and/or experience with this??



Thanks





Tom Parkinson - Quality System Manager - CIT

WinTronics, Inc.

Ph: 724-981-5770 Ext. 235

Fax: 724-981-1772






---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2