TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Date:
Wed, 2 Jun 2004 14:28:55 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Richard Kraszewski <[log in to unmask]>
Parts/Attachments:
text/plain (61 lines)
Nemi has an effort investigating the progress of industry standards
being updated for this purpose. 

ftp://nemi.org/webdownload/projects/ese/Assy%20Proc%20Standards_SOW1.pdf

Additionally from what I understand a similar issue was brought up at a
recent IPC-610C committee meeting.  

http://www.ipc.org/committeedetail.asp?Committee=7-31B

Rich Kraszewski 
Advanced Manufacturing Engineer - KEDS
Phone:  260.925.8919
 
 
 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Wednesday, June 02, 2004 12:14 PM
To: [log in to unmask]
Subject: [TN] Lead Free Solder Joint Requirements (Standards)


Fellow TechNetters & IPC

   Can some one shares with me or direct me to Lead free Solder Joint
Guidelines and/or Standards.   It has been my
personal observation from cross sections of LF Solder joint not to
exhibit the same lead wetting characteristics as SnPb
solder joints.   What is or will be the Acceptance Criteria for this new
family of solder joints.

   In advance I thank you for your timely response in this matter.

Victor,

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2