TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
Date:
Mon, 21 Jun 2004 08:35:56 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (184 lines)
I have found the following phrase to work well

"We would be happy to accommodate your request for this unique
manufacturing approach.  We do, however, charge a premium price for doing
things wrong".

Doug Pauls




                      "Whittaker, Dewey
                      (AZ75)"                     To:       [log in to unmask]
                      <Dewey.Whittaker@HON        cc:
                      EYWELL.COM>                 Subject:  Re: [TN] Customer Asking Not To Use Immersion Silver
                      Sent by: TechNet
                      <[log in to unmask]>


                      06/21/2004 08:03 AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      "Whittaker, Dewey
                      (AZ75)"







Dave,
I agree with George. I had a manager once tell me to never say no to a
customer. I have learned over the years to say yes to a customer in such a
way that he knows the answer is no.
Dewey

-----Original Message-----
From: Wenger, George M. [mailto:[log in to unmask]]
Sent: Friday, June 18, 2004 4:31 PM
To: [log in to unmask]
Subject: [TN] Customer Asking Not To Use Immersion Silver


Dave,

The advice you got from TechNeter about immersion silver is correct.
However, in all my years working in the telecommunications industry I've
learned three thinks about customers:

1. Listen to your customer. While your listening to them try to educate
them.

2. Listen to your customer.  When they don't hear what you are saying,
talk a little louder.

3. Listen to your customer.  And if they refuse to listen even when they
are wrong, do what they ask or they won't be your customer anymore.



Regards,
George
George M. Wenger, Andrew Corporation
Reliablity / FMA Engineer
Base Station & Subsystems Group
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Frank Kimmey
Sent: Friday, June 18, 2004 1:22 PM
To: [log in to unmask]
Subject: Re: [TN] Yellow Discoloration of Immersion Silver Boards

Dave,
Call me or Don Cullen if you need to but,

THERE IS NO REASON FOR CONCERN ABOUT MIGRATION WITH IMMERSION SILVER!!!

I took over 2 years in my investigation and qualification of IAg and
never once was able to document any migration.
Silver plate options can have grounds for concern, but not Immersion.
Unfortunately everyone knows someone who had a problem with Silver (but
no one has ever told me they personally have seen IAg migrate).

Talk to your PCB Supplier to get data from the correct IAg Supplier and
use that to teach your customer that the "old wives tale" is just that
and has no grounds for belief.

Hope it helps,
FNK

Frank N Kimmey CID+
Principle PCB Designer
Powerwave Technologies
EDH 916-941-3159
FAX 916-941-3195
CEL 916-804-2491


-----Original Message-----
From: Dave Chapman [mailto:[log in to unmask]]
Sent: Friday, June 18, 2004 10:03 AM
To: [log in to unmask]
Subject: Re: [TN] Yellow Discoloration of Immersion Silver Boards


I now have a customer asking us not to use Immersion Silver due to
migration. Isn't this old news? I thought the benzomidazole and other
organic inhibitors prevented Silver migration.
Dave C.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

----------------------------------------------------------------------------

--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
----------------------------------------------------------------------------

--------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2