If you test the raw board, you know how dirty it was. It you test a
populated board (and compensate the test results for the increased square
inches or cm) than you know the amount of 'dirt' on the board and the
components.
And it you believe in Murphy, you know that some of the dirt from the
components will ultimately get to the spot on the assembly where it will do
most harm.
Ahne.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Macko, Joe @ IEC
Sent: Thursday, June 10, 2004 12:36
To: [log in to unmask]
Subject: [TN] Surface Insulation Resistance (SIR) testing of populated
boards
Good Afternoon,
We are generating a test plan to evaluate the selection of a new saponifier
for our WESTEK in-line cleaner. We have been looking at running a SIR test
but most literature I read discusses running this test on bare boards and
not populated boards. Is there a reason for this? Would someone please
comment on the value of running this test on populated boards vs. bare
boards? thanks
joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|