TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 11 Jun 2004 13:20:20 +0200
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Daan Terstegge <[log in to unmask]>
Subject:
MIME-Version:
1.0 (Generated by Clearswift ES version 4.8.1.149)
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
From:
Daan Terstegge <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Hi Technet,

We've recently had delamination problems on boards which are populated
with some very expensive QFP's. To minimize the damage we want to
desolder these parts and use them again. Our customer wants some kind of
evidence that the functionality and long term reliability are not
affected, and they want this evidence (i.e. thermal profiles) to be
related to IPC specifications.

I'm not aware of any standard that specifies if reuse of desoldered
components is allowed, and which limitations apply to the temperature
profiles, but perhaps some of you knows such a standard ?

Best regards,

Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2