Hi folks! Don Cullen's committee (sorry, I forget the IPC task group
number) recently completed a very extensive electromigration test of
immersion silver as part of a UL acceptance/teaming exercise. Those test
results showed that the immersion silver did not migrate but the
electrolytic silver did. I recommend you contact John Perry for a copy of
the testing report. I have recently used the test data as topic information
in the "doesn't immersion silver migrate?" design team discussions.
Dave Hillman
Rockwell Collins
[log in to unmask]
Leo Higgins
<Leo_Higgins@ASAT To: [log in to unmask]
.COM> cc:
Sent by: TechNet Subject: Re: [TN] Immersion Silver finish and press-fit connectors
<[log in to unmask]>
06/10/2004 12:39
PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Leo
Higgins
Any concern for Ag migration since the Ag is not dissolved into solder...
------------------------------------
Leo M. Higgins III, Ph.D.
Director of Applications Engineering / ASAT Inc.
[log in to unmask]
3755 Capital of Texas Hwy-So
Suite 100
Austin, TX USA 78726
tel: 512-383-4593
fax: 512-383-1590
mobile: 512-423-2002
------------------------------------
-----Original Message-----
From: Whittaker, Dewey (AZ75) [mailto:[log in to unmask]]
Sent: Thursday, June 10, 2004 8:42 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion Silver finish and press-fit connectors
Craig,
Although Immersion Silver is a good choice for a lot of reasons, it would
be
the last choice compared to all the others for applications dealing with
press-fit or compliant pins(IMHO).
Dewey
-----Original Message-----
From: Craig Cullum [mailto:[log in to unmask]]
Sent: Wednesday, June 09, 2004 6:27 AM
To: [log in to unmask]
Subject: [TN] Immersion Silver finish and press-fit connectors
Hello all,
We are considering switching from HASL to Immersion Silver finsih on our
PCBs.
How would this impact the 2mm press-fit connectors?
Anyone willing to share their experiences?
Thank you in advance.
Regards,
Craig
Craig Cullum, Engineering Technologist, AMTELCO
e: [log in to unmask]
[log in to unmask]
f: 608 838 8367
v: 608 838 4194, or 4197, x128
Visit AMTELCO at www.amtelco.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|