Workmanship requirements are included within the 6012 specification. These
typically include fingerprints, scratches, and other cosmetic type issues.
If there are workmanship defects then they "may" not comply with the 6012
document.
Usually (this is written in there somewhere) these type defects are agreed
upon by supplier and customer.
Franklin
----- Original Message -----
From: "Mark Hargreaves" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, May 21, 2004 9:14 AM
Subject: [TN] conformance vs workmanship
> Hi All,
> May be a dumb question, but here goes:
> What's the difference (if any) between conformance to spec (ie. IPC6012
> class2) and workmanship? Can a bare board that conforms to the spec
exhibit
> poor workmanship (or visa versa)?
>
> Thanks,
> Mark Hargreaves
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|