I think this is from Mil S 13949 laminate spec which has now been withdrawn
& superseded by IPC4101.
I don't have a copy of 13949 but I'll take a shot at interpreting it.
GF = glass epoxy -flame resistant
.XXX = thickness in thou -sorry mils
C = copper clad
1/1 = 1 ounce double sided
A = Class of surface finish
1 = Thickness tolerance
Geoff Layhe
Lamar Group Ltd
-----Original Message-----
From: Craig Cullum [mailto:[log in to unmask]]
Sent: Friday, May 21, 2004 2:59 PM
To: [log in to unmask]
Subject: [TN] laminate specification (was RE: [TN] MIL-P-39949??)
Hello technetters,
A timely opportunity to ask a Friday question:
We are an OEM and have our PCBs fabricated outsourced locally.
On our older products the previous staff used the following spec
(example below) on our drill prints and I've always wanted an
interpretation:
4 layers TL-GF-.XXX-C-1/1-A1
Sometimes the "TL" is "FL". Specifically, what do these letters
REALLY mean? Is there an IPC or mil spec that spells this out?
Thanks all in advance. No rush.
Craig Cullum, Engineering Technologist, AMTELCO
e: [log in to unmask]
[log in to unmask]
f: 608 838 8367
v: 608 838 4194, or 4197, x128
Visit AMTELCO at www.amtelco.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
Private & Confidential:
This e-mail message is confidential and is intended solely for the person or
organisation to whom it is addressed. If the message is received by anyone
other than the addressee please return the message to the sender by replying
to it and then delete the message from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|