I installed the first OA (misnomer, WS is better) full scale
wave-soldering production line in Switzerland (if not in Europe) as long
ago as 1965. The company in question is still using it,four soldering
machines later. I have since aided in many others, throughout the world.
Advantages of WS:
- better quality soldering with fewer rejects
- more tolerant of poorly solderable components
- widest operating window
- no expensive cleaning products
- minimal pollution from overall process
- lowest production costs
Disadvantages:
- requires good process control
- unforgiving of errors
- good quality cleaning equipment rarer than you think
- flux itself is fairly corrosive
Summary:
- requires a serious approach and qualification
- with this proviso, this is the way to go.
Brian
Dehoyos, Ramon wrote:
> Hi Technetters:
> Has anybody done a comparison study of RMA/OA fluxes for wavesolder? Or any personal experiences in this regard will be appreciated.
> Thanks in Advance
> Ramon
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|